Results 1 to 2 of 2

Thread: Galvanized Capping

  1. #1
    Join Date
    May 2007
    Location
    in the wild New England, NSW
    Posts
    4,918
    Total Downloaded
    0

    Galvanized Capping

    Prior to painting a ute-back Ser 3 LWB, I have removed the gal cappings and would like to brighten the surface up as it has that white surface powdery finish now.

    Can it be acid/alkali bathed to restore ?

    Or is it better just to wire brush & etch prime it and then give it a coat of paint or cold gal?

    .... thanks - Laurie

  2. #2
    Join Date
    Aug 2006
    Location
    WA
    Posts
    13,786
    Total Downloaded
    0
    Best option is to get them re-galvanised.

    Otherwise, a wire brush/steelo and vinegar - or some weak acid. However by doing this you will be reducing the lifetime of the gal by a small amount.

    Phosphoric acid or undiluted degreaser will likely make it whiter.

Bookmarks

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Search AULRO.com ONLY!
Search All the Web!