No, didn't have any weaknesses in the length of the angles, just offset stitch welded every few inches and chamfered the ends (probably should have said open-ended). That way you can get a lot of paint inside and can hose them out if any mud gets in. I think that if a suitable duragal angle was available today I would use it and have the added protection of the plating. Used 3M tank sealant inside and Rust Guard paint on the outside.